Mori Silk
ENVIRONMENT
- The pulp is bleached using an Elementary Chlorine Free (ECF) process.
- Recyclable paper
- Recyclable packaging materials
Technical Specs
| Basis Weight |
Thickness |
Gloss |
Smoothness |
ISO Brightness |
Opactiy |
| g/m² |
mm |
% |
sec |
% |
% |
|
ISO 534 |
JIS P8142 |
J TAPPI No 5B |
ISO 2470 |
ISO 2471 |
| 105 |
0.090 |
29 |
1619 |
91 |
94 |
| 113 |
0.098 |
29 |
1518 |
92 |
95 |
| 128 |
0.115 |
31 |
1485 |
92 |
- |
| 150 |
0.113 |
30 |
1681 |
92 |
- |
| 170 |
0.162 |
26 |
1225 |
92 |
- |
| 210 |
0.214 |
28 |
1472 |
92 |
- |
| 256 |
0.258 |
37 |
1087 |
92 |
- |
| 300 |
0.309 |
36 |
1011 |
92 |
- |
| 350 |
0.371 |
36 |
902 |
91 |
- |
*measuring condition: temperature 23 ±1 °C, relative humidity 50 +/-±2%
*This Data only represents the actual value of most recent production. This does Not guarantee the standard quality